The metal reflet glaze samples were prepared with the Huxian wheat-meal-stone accession 0%, 5%, 10% and 15% according to the traditional metal reflet glaze formula and then sintered at 950%.
摘要在
属光泽

基础上,制作了4组户县麦饭石添量为0%,5%,10%,15%的
属光泽
试样,在950℃温度环境下烧成。
;
物;